Abstract
In this work, photoluminescence properties of the Y2O 3:Eu3+ nanophosphor was enhanced by applying newly developed pre-dispersing synthetic method with organic solvent. The particle size was smaller than 4 nm, and crystallinity of l(222)ll (511) was enhanced to 10.5. Also, using the 250 nm ultraviolet source, the highly intensive photoluminescence properties could be achieved at 611 nm with the pre-dispersing synthetic method with organic solvent.