Optimizing the Ag/Bi ratio for controlled growth of AgBiS2 thin films via a two-stage process

  • U. Chalapathi
  • , Kirakala Kiran Kumar
  • , Athipalli Divya
  • , Radhalayam Dhanalakshmi
  • , Krithikaa Mohanarangam
  • , Cuddapah Dhananjaya Rao
  • , Sambasivam Sangaraju
  • , C. Safarov Abduvahid Shukurovich
  • , Vasudevareddy Minnam Reddy
  • , Si Hyun Park
  • Termez State University
  • Apollo Hospitals Group
  • Universidad de Santiago de Chile
  • Symbiosis International University
  • Navoi State Pedagogical Institute
  • United Arab Emirates University
  • Saveetha Institute of Medical and Technical Sciences (Deemed to be University)
  • Yeungnam University

Research output: Contribution to journal › Article › peer-review

Abstract

This study focuses on synthesizing AgBiS2 thin films by sulfurizing Bi/Ag metal precursors in a graphite box. At a ratio of 1.26, Ag2S secondary phase was present, resulting in nonuniform grain growth, a 0.99 eV energy gap, and 640 Ω cm resistivity. Near-stoichiometric ratios (1.07 and 0.90) eliminated secondary phases, yielding phase-pure AgBiS2 with uniform grains, a 1.02 eV energy gap, and 13.7 Ω cm resistivity. At a 0.79 ratio, increased crystallinity and resistivity (25 Ω cm) were observed. These results highlight the importance of stoichiometry in fabricating high-quality AgBiS2 films for solar cells.

Original languageEnglish
Pages (from-to)596-603
Number of pages8
JournalJournal of Optoelectronics and Advanced Materials
Volume27
Issue number11-12
StatePublished - 1 Nov 2025

Keywords

  • AgBiS2
  • Evaporation
  • Thin films

Fingerprint

Dive into the research topics of 'Optimizing the Ag/Bi ratio for controlled growth of AgBiS2 thin films via a two-stage process'. Together they form a unique fingerprint.

Cite this